Volume:

0,65 kg

2,3 kg

Colour:

Product description
Characteristic
Video
Documents

Application - Призначення

It is intended to cover parquet floors, wood and metal products, as well as to add wood products decorative looks.

Advantages

The lacquer preserves perfectly the wood surface texture, forms a mirror luster, is resistant to abrasion and water impact, protects the surface against atmospheric effects.

Surface preparation 

Before the surface coating it should be thoroughly cleaned, sanded and scraped.

Lacquer preparation 

Lacquer should be stirred thoroughly. If it is necessary, it should be diluted with white spirit, thinner UETS, solvents, turpentine or with the mixture of the mentioned thinners in the ratio 1: 1.

Application methods 

The lacquer should be applied with a brush or a roller in 2-3 layers.

Guarantee storage life 

6 months from the production date

Lacquer consumption due to the timber spicies and the condition of surface treatmentfrom 60 g/m2 to 70 g/m2
Lacquer colour according to iodimetric scale100 mg l2 / 100 sm3 and less
Mass fraction of nonvolatile substances50±3%
Funnel viscosity by viscometer VZ-246 with nozzle diameter of 4 mm at temperature (20±2) °С-50-80 s
Time of the film full drying at temperature (20±2) °С6 h and less
The film hardness by pendulum device0,4 y.o.
Product description

Application - Призначення

It is intended to cover parquet floors, wood and metal products, as well as to add wood products decorative looks.

Advantages

The lacquer preserves perfectly the wood surface texture, forms a mirror luster, is resistant to abrasion and water impact, protects the surface against atmospheric effects.

Surface preparation 

Before the surface coating it should be thoroughly cleaned, sanded and scraped.

Lacquer preparation 

Lacquer should be stirred thoroughly. If it is necessary, it should be diluted with white spirit, thinner UETS, solvents, turpentine or with the mixture of the mentioned thinners in the ratio 1: 1.

Application methods 

The lacquer should be applied with a brush or a roller in 2-3 layers.

Guarantee storage life 

6 months from the production date

Characteristic
Lacquer consumption due to the timber spicies and the condition of surface treatmentfrom 60 g/m2 to 70 g/m2
Lacquer colour according to iodimetric scale100 mg l2 / 100 sm3 and less
Mass fraction of nonvolatile substances50±3%
Funnel viscosity by viscometer VZ-246 with nozzle diameter of 4 mm at temperature (20±2) °С-50-80 s
Time of the film full drying at temperature (20±2) °С6 h and less
The film hardness by pendulum device0,4 y.o.