Product description
Characteristic
Video
Documents
Enamel consumption for the first layer50-80 g/m²
Funnel viscosity by viscometer VZ-460-120 s
Mass fraction of nonvolatile substances62-72 %
Grinding degreenot more than 25 mkm
Dried film coating depending on colournot more than 100 g/m²
Time for complete drying at temperature (20±2) °Сnot more than 12 h
The film hardness by pendulum devicenot less than 0,25 у.о.
The film adhesionnot less than 1 ball
Product description
Characteristic
Enamel consumption for the first layer50-80 g/m²
Funnel viscosity by viscometer VZ-460-120 s
Mass fraction of nonvolatile substances62-72 %
Grinding degreenot more than 25 mkm
Dried film coating depending on colournot more than 100 g/m²
Time for complete drying at temperature (20±2) °Сnot more than 12 h
The film hardness by pendulum devicenot less than 0,25 у.о.
The film adhesionnot less than 1 ball